Skip to main navigation Skip to search Skip to main content

Fractographic insights into cracking mechanisms and microstructure

Research output: Contribution to journal › Article › peer-review

Original languageEnglish
Pages (from-to)851-860
Number of pages0
JournalFatigue and Fracture of Engineering Materials and Structures
Volume36
Issue number9
DOIs
Publication statusPublished - 2013

Keywords

  • fractography
  • high strength steel
  • intergranular fatigue
  • layer porosity
  • quasi-cleavage
  • tungsten alloys

Cite this